API 6D Monogram Licensed: No. 6D-1832
CE PED 2014/68/EU Module H: NB 2195
Oxy Oman Approved AML: OMN-QAC-862-002

Flanged Joint Leaking

The gasketed joint is the part of a valve installation most likely to leak, and the valve usually takes the blame.

Bolting procedureGasket materialThermal cyclingFacing condition
Gasket Seating Stress, Bolt Relaxation & Flange Rotation Diagram CAD
Gasket Seating Stress, Bolt Relaxation & Flange Rotation Diagram CADASME PCC-1 COMPLIANT
01 / OVERVIEW

Flanged Joint Leaking

The gasketed joint is the part of a valve installation most likely to leak, and the valve usually takes the blame.

02 / Symptom

What it looks like on site

A weep or drip at the valve flange, often after a thermal cycle or a shutdown.

03 / Causes

The causes, in order of likelihood

  • Insufficient or uneven bolt load. Tightening by feel, or in a sequence that does not compress the gasket evenly.
  • Gasket not suited to the temperature. A soft gasket in a hot joint relaxes, and the bolt load is lost.
  • Thermal cycling. The bolts, gasket and flanges expand differently, so the joint that was tight cold weeps hot.
  • Damaged or painted facing. A scored facing, or paint on the sealing surface, gives the gasket nothing to seal against.
  • Gasket reused. A compressed gasket does not recover, and reusing one is a reliable way to produce a weep.
04 / Standard

Bolting procedure is not optional

A flange joint is compressed by the bolts, and the load has to be applied evenly. Tightening round the circle in one pass loads one side first and can leave the opposite side under-loaded even when every bolt reads the correct torque.

The usual practice is a crossing pattern in several increments, with the final pass to the specified torque. Where the joint is critical, the bolt elongation or the gasket compression is controlled rather than the torque alone.

05 / Standard

Temperature changes the joint

On a hot line the joint has to be re-tightened after the first thermal cycle, because the initial cycle relaxes the gasket and redistributes the load. A joint that was correct at ambient is often loose once the line is at temperature.

Where the joint is repeatedly leaking after thermal cycles, the gasket material is the item to review. A graphite-based or spiral wound gasket behaves very differently from a soft sheet gasket in exactly this condition.

06 / Standard

Facing condition

The gasket seals against the flange facing, so the facing has to be clean, flat and free of damage. Paint on a facing is a leak path, and a radial score across the sealing surface is a path from the bore to the outside.

That is why facings and threads are masked during painting, and why the facing condition is worth checking on receipt rather than after installation.

07 / Reference

Leak By Cause

ItemDetailNote
Weeps after the first heat-upThermal relaxationRe-tighten to procedure after the first cycle
Weeps repeatedly, hot onlyGasket material not suited to the temperatureChange to a spiral wound or graphite gasket
Weeps at one bolt positionUneven load or a damaged facingRe-torque in a crossing pattern; inspect the facing
Weeps from commissioningPaint, score or a reused gasketClean the facing and fit a new gasket
Weeps on several joints at onceBolting procedureIntroduce a written tightening sequence
08 / Field checks

The checks, in order

01

Confirm the leak is at the joint

Distinguish a flange leak from a body joint or a packing leak.

02

Check the facing condition

Paint, scoring and corrosion on the sealing surface.

03

Review the gasket type against the temperature

The usual root cause on a joint that leaks hot.

04

Check the tightening sequence

Even load, crossing pattern, several increments.

05

Re-torque after the first thermal cycle

Standard practice on a hot line.

09 / Pictured

From the works and the projects

Hydraulic Bolt Tensioning and Flange Serration Inspection
Hydraulic Bolt Tensioning and Flange Serration InspectionCALIBRATED TORQUE
10 / FAQ

Questions this page answers

Because the bolts, gasket and flanges expand differently, and the gasket relaxes. Re-tightening after the first thermal cycle, and choosing a gasket suited to the temperature, are the usual fixes.

No. A compressed gasket does not recover, and reusing one is a reliable way to produce a weep. Replace it whenever the joint is broken.

Yes. Paint is a leak path and a compressible layer the gasket cannot seal against. Facings are masked during painting for exactly this reason.